{"_buckets": {"deposit": "9c0db392-906a-4666-a121-dfe8f016cd85"}, "_deposit": {"created_by": 3, "id": "6350", "owners": [3], "pid": {"revision_id": 0, "type": "depid", "value": "6350"}, "status": "published"}, "_oai": {"id": "oai:nifs-repository.repo.nii.ac.jp:00006350", "sets": ["17"]}, "author_link": ["117036", "117040", "117038", "117042", "117039", "117035", "117037", "117043", "117041"], "item_4_biblio_info_8": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicVolumeNumber": "Annual Report Apr.2008 - Mar.2009", "bibliographic_titles": [{}, {"bibliographic_title": "Annual Report of National Institute for Fusion Science", "bibliographic_titleLang": "en"}]}]}, "item_4_source_id_12": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0917-1185", "subitem_source_identifier_type": "ISSN"}]}, "item_4_start_page_10": {"attribute_name": "ページ", "attribute_value_mlt": [{"subitem_start_page": "436"}]}, "item_4_text_5": {"attribute_name": "所属", "attribute_value_mlt": [{"subitem_text_value": "NIFS"}]}, "item_4_text_9": {"attribute_name": "節", "attribute_value_mlt": [{"subitem_text_value": "11月2日"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "Kondo, M.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117035", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Nagasaka, T.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117036", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Sagara, A.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117037", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Muroga, T.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117038", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Oyama, D.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117039", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Nagura, M.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117040", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Suzuki, A.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117041", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Terai, T.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117042", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Fujii, N.", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "117043", "nameIdentifierScheme": "WEKO"}]}]}, "item_files": {"attribute_name": "ファイル情報", "attribute_type": "file", "attribute_value_mlt": [{"accessrole": "open_date", "date": [{"dateType": "Available", "dateValue": "2016-03-15"}], "displaytype": "detail", "download_preview_message": "", "file_order": 0, "filename": "ANREP08-09-436.pdf", "filesize": [{"value": "134.8 kB"}], "format": "application/pdf", "future_date_message": "", "is_thumbnail": false, "licensetype": "license_free", "mimetype": "application/pdf", "size": 134800.0, "url": {"label": "ANREP08-09-436.pdf", "url": "https://nifs-repository.repo.nii.ac.jp/record/6350/files/ANREP08-09-436.pdf"}, "version_id": "1fabb65a-0e52-40dd-9dd8-809c4d1e37ac"}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "eng"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "departmental bulletin paper", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "Corrosion Characteristics of Reduced Activation Ferritic Steel, JLF-1(8.92Cr-2W) in Molten Salts Flibe and Flinak", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "Corrosion Characteristics of Reduced Activation Ferritic Steel, JLF-1(8.92Cr-2W) in Molten Salts Flibe and Flinak", "subitem_title_language": "en"}]}, "item_type_id": "4", "owner": "3", "path": ["17"], "permalink_uri": "http://hdl.handle.net/10655/4900", "pubdate": {"attribute_name": "公開日", "attribute_value": "2011-01-27"}, "publish_date": "2011-01-27", "publish_status": "0", "recid": "6350", "relation": {}, "relation_version_is_last": true, "title": ["Corrosion Characteristics of Reduced Activation Ferritic Steel, JLF-1(8.92Cr-2W) in Molten Salts Flibe and Flinak"], "weko_shared_id": -1}
Corrosion Characteristics of Reduced Activation Ferritic Steel, JLF-1(8.92Cr-2W) in Molten Salts Flibe and Flinak
http://hdl.handle.net/10655/4900
http://hdl.handle.net/10655/4900ec7bf81b-bd10-4d82-864e-0911971eae76
名前 / ファイル | ライセンス | アクション |
---|---|---|
ANREP08-09-436.pdf (134.8 kB)
|
|
Item type | 紀要論文 / Departmental Bulletin Paper_02(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2011-01-27 | |||||
タイトル | ||||||
言語 | en | |||||
タイトル | Corrosion Characteristics of Reduced Activation Ferritic Steel, JLF-1(8.92Cr-2W) in Molten Salts Flibe and Flinak | |||||
言語 | ||||||
言語 | eng | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | departmental bulletin paper | |||||
著者 |
Kondo, M.
× Kondo, M.× Nagasaka, T.× Sagara, A.× Muroga, T.× Oyama, D.× Nagura, M.× Suzuki, A.× Terai, T.× Fujii, N. |
|||||
所属 | ||||||
NIFS | ||||||
書誌情報 |
en : Annual Report of National Institute for Fusion Science 巻 Annual Report Apr.2008 - Mar.2009 |
|||||
節 | ||||||
11月2日 | ||||||
ページ | ||||||
開始ページ | 436 | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0917-1185 |